Image is for reference only, refer to product info for complete details.
Designed for mixing two-part high-temperature ceramic cement, this tan powder filler combines with the matching liquid binder to form a ceramic bond rated to 1550°F (843°C). It is supplied in 8 oz. Great for bonding thermocouples and heating elements and electrically insulating sensor leads.
Designed for mixing two-part high-temperature ceramic cement, this tan powder filler combines with the matching liquid binder to form a ceramic bond rated to 1550°F (843°C). It is supplied in 8 oz. Great for bonding thermocouples and heating elements and electrically insulating sensor leads.
Chemical set cements set or cure by an internal chemical action which does not require exposure to air. Chemical set cements can be used in thick applications (applied in thicknesses greater than 1/4").
Features
Applications
| Type of cement (1 or 2 Part) | 2 part |
| Coefficient of thermal expansion | 4.6 x 10-6"/in/°F |
| Color | Tan |
| Compressive strength | 3900 psi |
| Density | 141 lb/ft3 |
| Dielectric constant | 5.0 to 7.0 |
| Dielectric strength at 20°C (70°F) | 25.0 to 51.0 V/mil |
| Dielectric strength at 400°C (750°F) | 12.5 to 25.0 V/mil |
| Dielectric strength at 795°C (1475°F) | ≤1.3 V/mil |
| Maximum service temperature | 1550°F (843°C) |
| Volume resistivity at 20°C (70°F) | 107-109 Ω-cm |
| Volume resistivity at 400°C (750°F) | 104-106 Ω-cm |
| Volume resistivity at 795°C (1475°F) | 102-103 Ω-cm |
| Absorption | 10 - 12% |
| Shrinkage | 0.5% |
| Thermal conductivity | 8 Btu-in/ft2-hr-°F |
| Mix ratio | Mix 3 parts powder to 1 part liquid by weight, or 2 parts filler to 1 part liquid by volume |
| Description | CC high temperature cement powder, 8 oz by weight (2 part cement; mix liquid with CC binder) |
| Type of cement (1 or 2 Part) | 2 part |
| Coefficient of thermal expansion | 4.6 x 10-6"/in/°F |
| Color | Tan |
| Compressive strength | 3900 psi |
| Density | 141 lb/ft3 |
| Dielectric constant | 5.0 to 7.0 |
| Dielectric strength at 20°C (70°F) | 25.0 to 51.0 V/mil |
| Dielectric strength at 400°C (750°F) | 12.5 to 25.0 V/mil |
| Dielectric strength at 795°C (1475°F) | ≤1.3 V/mil |
| Maximum service temperature | 1550°F (843°C) |
| Volume resistivity at 20°C (70°F) | 107-109 Ω-cm |
| Volume resistivity at 400°C (750°F) | 104-106 Ω-cm |
| Volume resistivity at 795°C (1475°F) | 102-103 Ω-cm |
| Absorption | 10 - 12% |
| Shrinkage | 0.5% |
| Thermal conductivity | 8 Btu-in/ft2-hr-°F |
| Mix ratio | Mix 3 parts powder to 1 part liquid by weight, or 2 parts filler to 1 part liquid by volume |
| Description | CC high temperature cement powder, 8 oz by weight (2 part cement; mix liquid with CC binder) |